Parker LORD Structural Adhesives, Thermal Management & Electronic Materials
Parker LORD develops engineered materials for structural bonding, thermal management, semiconductor and electronic assembly, surface preparation, and elastomer bonding. The portfolio includes LORD epoxy, structural acrylic, urethane, and specialty adhesive systems; COOLTHERM materials for thermal management and electronic packaging; and Chemlok materials for rubber-to-substrate bonding.
As an authorized Parker LORD distributor, Krayden supplies a selection of structural adhesives, COOLTHERM thermal-management and electronic materials, Chemlok bonding systems, and related surface-preparation products. Our team can help customers compare adhesive chemistry, substrates, bond or gap geometry, thermal requirements, dispensing methods, cure processes, electrical requirements, and other application-specific considerations.
Markets Served by Parker LORD
Featured Parker LORD Brands
Key Parker LORD brands supporting structural bonding, thermal management, electronic packaging, and rubber-to-substrate bonding.
LORD
Structural adhesive systems spanning epoxy, structural acrylic, urethane, and specialty chemistries for engineered assembly. Product selection depends on substrates, bond geometry, cure and handling requirements, and the mechanical demands of the finished assembly.
COOLTHERM
Thermal-management and electronic materials including thermally conductive adhesives, gap fillers, gels, potting and encapsulation systems, die-attach materials, and semiconductor-package protection products.
Chemlok
Elastomer-bonding materials for rubber-to-metal and rubber-to-substrate applications, including systems used during molding and specialized bonding processes.
Structural Adhesives
Parker LORD structural adhesives include epoxy, structural acrylic, urethane, and specialty systems for joining metals, composites, plastics, and other engineered assemblies. Different chemistries address different combinations of cure speed, stiffness or flexibility, gap filling, impact and peel requirements, substrate preparation, and production method.
Thermal Management Materials
COOLTHERM materials support thermal interfaces and component protection in EV batteries, power electronics, motors, semiconductor assemblies, and other heat-generating systems. The portfolio includes thermally conductive adhesives, dispensable gap fillers, gels, and potting or encapsulation systems.
Rubber-to-Substrate Bonding
Chemlok bonding systems are used to bond rubber and other elastomers to metal and selected rigid substrates during molding, curing, and specialized post-vulcanization processes. Product selection depends on elastomer type, substrate, molding conditions, cure temperature, surface preparation, and required environmental resistance.
Electronic Assembly & Semiconductor Packaging
Parker LORD electronic materials support semiconductor die attachment, package underfill, encapsulation, and related electronic assembly requirements. Selection depends on package architecture, thermal and electrical requirements, cure conditions, flow behavior, coefficient-of-thermal-expansion considerations, reliability targets, and manufacturing process.
Surface Preparation Materials
Parker LORD surface-preparation materials include primers, accelerators, and adhesion promoters used with selected adhesive and elastomer-bonding processes. These products should be matched to the exact adhesive system, substrate condition, cleaning method, and production sequence.
Primers
Primers condition properly prepared substrates before selected adhesive or elastomer-bonding processes. The correct primer depends on substrate, adhesive chemistry, cleaning process, coating method, and drying requirements.
Accelerators
Accelerators are paired with specified LORD adhesive systems to initiate or influence cure behavior. Working time, production cycle, application sequence, and adhesive compatibility should be confirmed for the selected system.
Adhesion Promoters
Adhesion promoters and surface treatments improve receptivity of selected plastics, rubbers, and other difficult substrates when used with compatible bonding systems and the specified surface-preparation process.
Talk to our Experts
Krayden can help compare Parker LORD materials for structural bonding, thermal management, electronic assembly, elastomer bonding, surface preparation, and related manufacturing requirements. Our team can support product selection, substrate and application review, processing considerations, and comparison of candidate materials for your production needs.
Parker LORD Quick Reference
164 products
-
LORD 7545
- 1:1 mix ratio, 100% solids urethane adhesive
- 1.5 to 65 minute selectable working time
- Non-sag structural bonding with environmental and solvent resistance.
-
COOLTHERM EP-6972
- <0.0005 ohm-cm Volume Resistivity
- 2.13 W/(m K) Thermal Conductivity
- 1:1 Weight Mixing
-
COOLTHERM 6053
- Flexible Cured Material
- Heat & Oxidation Resistance
- Supplied in a 16-Ounce Aerosol Format
-
COOLTHERM 6250
- 350 cP Low-Viscosity Curing Agent
- High-Solids Adhesive/Encapsulation Curing Agent
- Chemical-Resistant Cured Epoxy Systems
-
COOLTHERM 6732
- Hardener Component Thermal Interface Material
- 100:0.5 Controlled Mixing
- Thermally Conductive Thermal Interface
-
COOLTHERM 6733
- Solvent-Free RTV Silicone Encapsulation
- Low-Stress No-Exotherm Room-Temperature Cure
- -60 to 205 deg C Continuous Service
-
COOLTHERM EP-6010
- 55 cP Application Viscosity
- Low-Shrinkage Epoxy Curing Agent
- Two-Year Shelf Life at 25 deg C
-
-
COOLTHERM PC10882
- Screen-Printable Coating Application
- Thermal-Shock and Solvent-Resistant Cured Film
- Above 500 V/mil Dielectric Strength
-
COOLTHERM SC-6730
- Room-Temperature Thick-Section Cure
- 3.0 to 10.0% Mix Concentration
- Blue-Green Visual Mix Indicator
-
LORD 304-2
- High-Viscosity Placement Control
- Rubber, Wood, and FRP Bonding
- Durable Cured Performance with Environmental
-
-
LORD 4688
- Low-Density Honeycomb-Core Syntactic Reinforcement
- Thixotropic Application Control
- 30-Minute Working Window
-
LORD 7100A
- High-Strength Structural Bonding
- Primerless Bonding to Many Plastics
- VOC-Free Weathering/Aging-Resistant Urethane
-
LORD 7100A/B
- High-Strength Structural Bonding
- Without Priming Bonding
- Solvent-, Weathering- and Aging-Resistant Cured System
-
LORD 7100B
- High-Strength Urethane Bonding
- Primerless Bonding to Many Plastics
- VOC-Free Weathering/Aging-Resistant Urethane
-
LORD 3135-B
- Former Lord 7111-B Hardener
- Low-Shrinkage Epoxy Bonding
- Room-Temperature or Accelerated Heat Curing
-
LORD 7150A/B
- High-Strength Structural Bonding
- Primerless Bonding to Many Plastics
- Solvent-, Weathering- and Aging-Resistant Gray Cured System
-
-
-
LORD 7542C
- 1:1 Medium-Work-Time Urethane Curative
- 10 to 20-Minute Working Time
- 60 to 120-Minute Handling Time
-
-
LORD 7545A/D
- High-Strength Structural Bonding
- Non-Sag Vertical Placement
- Solvent and Weather Resistance
-
LORD 7550
- Optically Clear Bonding
- 3 to 5-Minute Working Window
- Weathering/Humidity/Salt-Spray/UV Environmental Resistance
-
LORD 7650
- One-Part Moisture-Cure Urethane
- 15 to 30-Minute Solvent Flash
- Multi-Material Foam/Fabric/Rubber/Plastic/Metal Bonding
-
LORD 7800
- Rapid-Cure Urethane Bonding
- Composite, SMC, Plastic, and Coated-Metal Bonding
- Non-Sag Environmental Resistance
-
LORD ACCELERATOR 19GB
- Integrated 0.01 in (0.025 cm) Glass Beads
- Room-Temperature Curing Paste Material
- Non-Flammable Application Formulation
-
-
COOLTHERM EP-6252
- Defined Epoxy Hardener Component
- Electrical Encapsulation System Use
- Component-Level Metering Control
-
-
COOLTHERM EP-6011
- Hardener for Thermally Conductive Adhesive
- EP-6006 HS System Pairing
- Current-Carrying Conductor Bonding
-
COOLTHERM MT-125
- 2.35 W/(m K) Thermal Conductivity
- 21 MPa Aluminum Lap Shear
- Two-Week Working Life at 25 deg C
-
-
LORD 2232
- 425 cP Application Viscosity
- At Most 0.100 ohms/sq/mil Cured Resistivity
- 2- to 3-Second Solder Wetting
-
LORD 307-2
- 20,000 to 57,000 cP Hardener Viscosity
- 1:1 General-Purpose Volume Mix
- 1- to 2-Hour System Working Time
-
LORD 312-B
- 0.96 g/cm^3 Hardener Density
- 0.00% Volatile Content by Weight
- Potting and Thin-Film Encapsulation
-
-
-
LORD 7450
- Cryogenic Flexible Bonding
- Multifunction Adhesive and Sealant
- Room-Temperature or Accelerated Cure
-
LORD 7545-A
- Multi-Curative Work-Time Flexibility
- Equal-Volume System Mixing
- Manual or Automated Dispensing
-
LORD 7545-B
- 3 to 5 Minute A/B Work Time
- 30-Minute A/B Handling Strength
- Non-Sag A/B Vertical Placement
-
LORD 7545-C
- 6 to 8 Minute A/C Work Time
- 60-Minute A/C Handling Strength
- Non-Sag A/C Vertical Placement
-
LORD 7545-D
- 11 to 18 Minute A/D Work Time
- 90-Minute A/D Handling Strength
- Non-Sag A/D Vertical Placement
-
LORD 7545F
- 45 to 65 Minute A/F Work Time
- Manual or Automated A/F Dispensing
- Non-Sag A/F Vertical Placement
-
-
-
-
LORD PC-10678HV
- Flexible-Substrate Screen Printing
- Highly Conductive Grid Formation
- One-Component Paste Processing
-
COOLTHERM ME-543
- 21,000 cP Jet-Dispense Viscosity
- 7 to 20 Minute Cure at 160 to 165 deg C
- 260 deg C Peak Reflow Resistance
-
LORD 410/19 GB
- Acrylic Metal/Engineered-Plastic Structural Adhesive
- 20 to 30-Minute Working Window
- 18.6 MPa Cured Tensile Strength
-
LORD® 810S/20GB Flexible Acrylic Adhesive System
- 2:1 mix ratio acrylic adhesive system
- 8-12 minute selectable working time
- Non-sag structural bonding with environmental and solvent resistance.
-
-
COOLTHERM SC-6754
- 0.5 W/(m K) Thermal Conductivity
- Nil Bleed After 24 Hours at 200 deg C
- -55 to +205 deg C Continuous Service
-
COOLTHERM SC-3500
- 3.5 W/(m K) Thermal Conductivity
- <100 ppm Cyclic Siloxane Content
- 1:1 Weight or Volume Mixing
-
COOLTHERM TC-404
- 4.3 W/(m K) Thermal Conductivity
- 212,400 cP Viscosity
- Reworkable Non-Curing Interface
-
COOLTHERM TC-501
- 25 to 50 um Installed Bondline
- 3.6 W/(m K) Thermal Conductivity
- 24-Hour Working Life at 25 deg C
-
-
COOLTHERM MG-122
- Single-Component No-Mix Dispensing
- Thermally Conductive Chip Interface
- Flip-Chip and BGA Application Fit
-
COOTHERM CIRCALOK 6037
- Thermally Conductive Bonding
- 500,000 cP Resin Viscosity
- 1.2 W/(m K) Thermal Conductivity
-
LORD 403
- LORD Accelerator 17/19/19GB Compatibility
- Alternative to Welding/Brazing/Fastening
- Acrylic Adhesive with Multiple Accelerators
-
-
LORD 406
- Medium-Work-Time Acrylic Adhesive
- 6 to 10-Minute Working Window
- 18.6 MPa Cured Tensile Strength
-
LORD 406/19GB
- 4:1 Metal-to-Plastic Bonding
- 6 to 10-Minute Working Window
- 18.6 MPa Cured Tensile Strength
-
LORD 506
- 4 to 6-Minute Working Window
- Flexible Cured Adhesive
- Environmental Resistance Acrylic Bonding
-
-
LORD 850S/25GB
- Welding/Fastener Replacement Bonding
- 6 to 10-Minute Working Time
- Documented Chemical/Moisture/Salt-Spray/Weather Resistance
-
LORD 852/25GB
- Welding/Fastener Replacement Bonding
- 20 to 25-Minute Working Time
- Prepared/Unprepared Metal/FRP/Plastic Bonding
-
-
COOLTHERM 6410
- 600 cP Mixed Viscosity
- Flexible Encapsulation Protection
- Room-Temperature Encapsulation Cure
-
-
COOLTHERM 6735
- Eight-Hour Working Window
- 55 to 205 deg C Service Range
- Reversion-Resistant Addition-Cure System
-
-
CHEMLOK 7701
- Under Five-Minute Solvent Flash-Off
- No-Mix Surface Conditioning
- Wipe, Brush, Dip or Flood
-
COOLTHERM DC-812
- Automotive Encapsulation Application
- 1.4 x 10^16 ohm-cm Volume Resistivity
- Resistance to Thermal Shock and Electrical Stability
-
COOLTHERM E-105
- Clear Unfilled Epoxy Resin
- 600 cP Resin Viscosity
- Multiple CoolTherm/Circalok Hardener Compatibility
-
CHEMLOK 607
- Clear One-Coat Silicone-Elastomer Bonding
- Brush, Spray, or Dip Application
- Extreme-Temperature Elastomer Bond Systems
-
COOLTHERM EP-2000
- 1.9 W/(m K) Thermal Encapsulation
- 1,900 cP Mixed Viscosity
- 204 deg C Glass Transition
-
COOLTHERM EP-301
- 1.3 W/(m K) Thermal Encapsulation
- High-Fluidity Intricate-Circuitry Potting
- 19.7 kV/mm Dielectric Strength
-
COOLTHERM EP-340
- 1.5 W/(m K) Thermal Interface
- 7,000 to 60,000 cP Mixed Viscosity
- Low Cured Coefficient of Linear Thermal Expansion
-
COOLTHERM 6756
- Adhesion-Promoting Surface Treatment
- 1 cP Application Viscosity
- Recommended 3 to 10 um Film Thickness
-
COOLTHERM EP-3500
- 3.3 W/(m K) Thermal Conductivity
- 10.4 to 12 ppm/deg C CTE
- 205 to 206 deg C Glass Transition
-
-
COOLTHERM EP-6009
- 2,600 cP Mixed Viscosity
- 0.7 W/(m K) Thermal Encapsulation
- Electrically Insulating Encapsulation
-
COOLTHERM EP-6035
- 1.0 W/(m K) Thermal Encapsulation
- 12,000 cP Mixed Viscosity
- UL 94 V-0 Classification
-
COOLTHERM EP-6037
- 1.2 W/(m K) Thermal Conductivity
- Two Hardener Options for Controlled CTE
- Room-Temperature Adhesive Cure
-
COOLTHERM EP-636
- 205 deg C Staged-Cure Encapsulation
- 18.3 kV/mm Dielectric Strength
- 50,000 cP Mixed Viscosity
-
COOLTHERM ES-40
- Eight Configurable Hardener Options
- Adhesive, Laminating, and Electrical-Insulation Uses
- Up to 77.2 MPa Tensile Strength
-
-
COOLTHERM ME-531
- 4,000 cP Jettable Capillary Underfill
- 140 deg C Glass Transition
- 30-Minute 150 deg C Cure
-
COOLTHERM SC-104
- 0.8 W/(m K) Thermal Encapsulation
- 7,000 cP Mixed Viscosity
- 17.3 kV/mm Dielectric Strength
-
-
COOLTHERM SC-303
- 0.9 W/(m K) Thermal Conductivity
- 6,000 cP Application Viscosity
- 40 to 200 deg C Service Range
-
COOLTHERM SC-6702
- 0.7 W/(m K) Silicone Encapsulation
- 4-Hour Working Life
- -55 to 260 deg C Material Use
-
COOLTHERM SC-6703
- 0.8 W/(m K) Thermal Encapsulation
- 8,000 cP Mixed Viscosity
- 19.7 kV/mm Dielectric Strength
-
COOLTHERM SC-6705
- 55 to 205 deg C Service Range
- 2,500 cP Mixed Viscosity
- 17.7 kV/mm Dielectric Strength
-
COOLTHERM SC-6709
- 1.0 W/(m K) Thermal Encapsulation
- Three Hardener Options
- 68 to 205 deg C Service Range
-
COOLTHERM SC-6710
- 1.0 W/(m K) Thermal Encapsulation
- 20,000 cP Red Resin with Sc-6730 Processing
- 19.7 kV/mm Dielectric Strength
-
COOLTHERM SC-6711
- 1.0 W/(m K) Thermal Encapsulation
- 30,000 cP White Silicone Resin
- 19.7 kV/mm Dielectric Strength
-
COOLTHERM SC-6714
- UL 94 V-0 Encapsulation
- 55 to 205 deg C Service Range
- Circalok 6730/6731 Catalyst Compatibility
-
COOLTHERM SC-6725
- 1.16 W/(m K) Thermal Encapsulation
- 15,000 cP Mixed Viscosity
- Primerless Encapsulation Processing
-
COOLTHERM SC-6731
- 100 cP Resin Viscosity
- Concentrations from 0.1% to 5% by Weight
- Two-Component RTV Silicone Systems Used in Potting
-
-
-
-
COOLTHERM SC-309
- 0.9 W/(m K) Thermal Encapsulation
- Low-Viscosity Automated Meter-Mix Processing
- Room- or Heat-Cure Flexibility
-
LORD MAXLOK MX/T3S
- Minimal-Preparation Metal Bonding
- Fast 6- to 8-Minute Handling
- Controlled Non-Sag Bondline
-
COOLTHERM MT-322
- 1.7 W/(m K) Thermal Conductivity
- One-Month Working Life at 25 deg C
- -40 to +200 deg C Service Range
-
LORD 459X
- Adhesion-Promoting Surface Treatment
- Low-Viscosity Adhesive Application
- Brush, Dip or Spray Application
-
LORD 7701
- Cured-Rubber/Urethane/Elastomer Adhesion Treatment
- No-Mix Wipe/Brush/Dip/Flood Application
- Compatible LORD Epoxy/Urethane Adhesives
-
LORD AP-134
- One-Coat Moisture-Cure Multi-Substrate Primer
- No-Mix Spray/Dip/Felt Application
- 1 to 2-Hour Ambient Hydrolysis
-
-
LORD P-1292
- Platinum-Cure RTV Adhesion Promotion
- Broad-Substrate Addition-Cure Silicone Adhesion
- Hydrolytically Stable Silicone Bonding
-
COOLTHERM EP-6007
- 45-Minute Working Window
- 0.62 W/(m K) Thermal Interface
- 19.7 kV/mm Dielectric Strength
-
COOLTHERM SC-320
- 3.0 W/m·K thermal conductivity
- Low-stress, low-viscosity silicone
- UL 94 V-0 and Class H insulation
-
COOLTHERM SC-324
- 4.0 W/m·K thermal conductivity
- Durable UL 94 V-0 flame rated, addition-cure PDMS
- Low-stress low viscosity potting
-
COOLTHERM 6055
- Convenient 1:1 Volume Mixing
- Room-Temperature or Accelerated Cure
- Dielectric Epoxy Encapsulation
-
COOLTHERM 6408 6408 A SLW/B
- Extended 20-30 Minute Work Life
- High-Elongation Cured Protection
- Electrical Insulation for Encapsulation
-
COOLTHERM SC-6715
- Multiple Hardener Pairing Options
- Automatic Meter-Mix-Dispense Application
- Dense-Component Potting Resin
-
COOLTHERM 6716
- 45-Minute Mixed Working Window
- 100:2.5 Resin-Hardener Ratio
- Low- and High-Voltage Encapsulation
-
COOLTHERM 6744
- Low-Viscosity 1:1 Processing
- Two-Hour Room-Temperature Cure
- Flame-Retardant Silicone Encapsulation
-
COOLTHERM EP-6028
- 1:1 Resin-Hardener Mixing
- High-Voltage Transformer Potting
- 3-4 Hour System Heat Cure
-
COOLTHERM ES-21
- 35,000 cP Dispensing Viscosity
- UV Fluorescence for In-Line Inspection
- 60-Minute Cure at 125 deg C
-
COOLTHERM SC-252
- 2.5 W/(m K) Thermal Conductivity
- 8.7 kV/mm Dielectric Strength
- 1:1 Weight or Volume Mixing
-
-
COOLTHERM SC-6709/SC-6731
- 100:0.5 Weight Mixing
- 12 to 16 Hour Room-Temperature Cure
- 21.7 kV/mm Dielectric Strength
-
COOLTHERM SC-6717
- 17,000 cP Resin Viscosity
- 8 to 24 Hour Room-Temperature Cure
- 19.7 kV/mm Dielectric Strength
-
COOLTHERM SC-6726
- 3 to 5 Day Working Life at 25 deg C
- 1:1 Weight or Volume Mixing
- -55 to +200 deg C Operating Range
-
-
COOLTHERM UR-388
- UL 94 V-0 Classification
- 0.7 W/(m K) Thermal Conductivity
- 15.0 kV/mm Dielectric Strength
-
-
-
-
LORD 506/17
- 8-12 Minute Handling Strength
- 10:1 Accelerator 17 Volume Mix
- -40 to 149 deg C Temperature Range
-
LORD 606
- 5-7 Minute Mixed Working Window
- 10:1 Accelerator 17 Volume Mix
- DCPD Composite-to-Metal Bonding
-
LORD 661/6
- Up to 25.4 mm Gap Fill
- 11-19 Minute Working Window at 32 deg C
- 45-55 Minute Handling Strength
-
-
-
-
-
-
-
-
LORD 304-1
- High-Viscosity Placement Control
- Rubber, Wood, and FRP Bonding
- Durable Cured Performance with Environmental
-
LORD 305-1
- Medium-Viscosity Application Control
- Rubber-to-Wood Epoxy Bonding
- Chemically, Environmentally and Temperature Resistant
-
LORD 305-1/2
- Medium-Viscosity Application Control
- Rubber-to-Wood Epoxy Bonding
- Chemically, Environmentally and Temperature Resistant
-
LORD 305-2
- Medium-Viscosity Application Control
- Rubber-to-Wood Epoxy Bonding
- Chemically, Environmentally and Temperature Resistant
-
LORD 306-1
- High-Viscosity Non-Sag Gap Filling
- Documented Chemical/Moisture/Weather Resistance
- MIL-A-24456 Compliance Scope
-
LORD 3135
- Broad Multi-Material Structural Bonding
- Low-Shrinkage Epoxy System
- Documented NASA/MMM-A-134/MIL-A-8623A Compliance
-
LORD 3170
- Bond Strength Down to -253 deg C
- Low-Outgassing Aerospace Epoxy
- Equal-Volume Room-Temperature Cure
-
LORD 320
- Primerless Automotive-SMC Adhesion
- -40 to 204 deg C Service Range
- Solvent-Free Nonflammable Epoxy
-
LORD 320/310B
- Two-Component Epoxy for Treated Cured Rubber
- 30 to 60-Minute Working Window
- Durability Under Humidity Bonding
-
LORD 320/322
- Primerless Automotive-SMC Adhesion
- -40 to 204 deg C Service Range
- Solvent-Free Nonflammable Epoxy
-
LORD 322
- General-Purpose Two-Component Epoxy for SMC
- 20 to 40-Minute Working Window
- 30.6 MPa Cured Tensile Strength
-
LORD 363
- 3 to 5-Minute Working Window
- Self-Leveling Flowable Placement
- Solvent-Free Bonding Formulation
-
-
LORD 312-A
- 1.13 g/cm^3 Resin Density
- 0.00% Volatile Content by Weight
- Potting and Thin-Film Encapsulation
-
LORD 7550A Urethane Adhesive
- Equal-Mix LORD 7550 Resin Component
- 1,800 to 4,000 cP Viscosity
- Lexan, ABS, and Primed-Metal Bonding
-
LORD 7550C Urethane Adhesive
- Equal-Mix LORD 7550 Curative Component
- 6,000 to 12,500 cP Viscosity
- Lexan, ABS, and Primed-Metal Bonding
-
-
COOLTHERM 6027
- Fast Heat-Cure Processing
- Non-Sag Thixotropic Dispensing
- High-Resistivity Cured Insulation
-
COOLTHERM EP-6151
- Thermally Conductive Heat-Sink Bonding
- Fast High-Temperature Cure
- Shape-Holding Thixotropic Dispensing
-
-
-