SAC305 | Pb-free Solder Spheres

Harmonization Code : 8001.20 | Unwrought tin: Tin alloys

PMTC SAC305 Pb-free Solder Spheres SAC305 Pb-free Solder Spheres PMTC SAC305 Pb-free Solder Spheres

Main features

  • Leadfree Solder Spheres
  • Lowest cost Sn/Ag/Cu Alloy
  • Excellent Fatigue Resistance

Product Description

LINQALLOY SAC305 solder Spheres are lead-free Tin/Silver/Copper alloys that contain 96.5% Tin (Sn), 3% Silver (Ag), and 0.5% Copper (Cu) and is often written as Sn96.5Ag3.0Cu0.5. SAC305 Solder Spheres are the least expensive of the two industry standard lead-free solder spheres (the other being SAC405) and are used by companies working with BGA, CSP, LBGA, PBGA and CBGA components who have made the transition to Lead-free (Pb-free) soldering.

Features:

  • Lowest Cost Sn/Ag/Cu Alloy
  • Excellent Fatigue Resistance
  • Compatible with all Flux Types
  • Excellent Solder Joint Reliability
  • Best Wetting Sn/Ag/Cu Alloy

Each jar has a clear label on the lid specifying the solder ball diameter as well as a label on the front identifying the alloy type, the quantity of spheres in the jar, the date of manufacture, and the product lot (or batch) number. This batch number is also tied to a certificate of conformance that is also provided with the solder spheres and ensures the SAC305 solder spheres meet the following quality criteria:

  • Tin (Sn): 96.5%
  • Silver (Ag): 3%
  • Copper (Cu): 0.5%
  • Melting Temperature (Solidus): 217°C
  • Melting Temperature (Liquidus): 219°C
  • Sphericity : Within 1.5%

Diameter Tolerance

  • 0.22mm - 0.48mm (220µm - 480µm) : ± 0.010mm (± 10µm)
  • 0.50mm - 0.762mm (500µm - 762µm) : ± 0.025mm (± 25µm)
Product Family

230948

Alloy: Sn96.5/Ag3.0/Cu0.5 » 0.075mm (3mil) » 250,000 spheres
1. Select Diameter
2. Select Package Size

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Unit of measure Jar
Net weight 0.0004 kg
Gross weight 0.0004 kg
Dimensions 6 x 6 x 10 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Alloy Composition
Composition of the alloy material
Sn96.5Ag3.0Cu0.5
Alloy Type
A metallic element type
SAC305
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
7.4g/cc
Other Properties
RoHS Compliant
RoHS is a product level compliance based on a European Union Directive which restricts the Use of certain Hazardous Substances in Electrical and Electronic Equipment (RoHS). Products compliant with this directive do not exceed the allowable amounts of the following restricted materials: lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls (PBB) and polybrominated diphenyl ethers (PBDE), with some limited exemptions
Yes

Additional Information

SAC 305 Reflow profile

Preheating Stage

Soaking Stage

Reflow Stage

Cooling Stage

Preheat Rate [ºC/s]  

Preheat Temperature [ºC]

Soaking time [s]

Soaking Temperature [ºC]

Reflow time [s]

Peak Temperature [ºC]

Cooling Rate [ºC/s] 

1.0 - 3.0

170

60 — 70 

170 — 180

45 — 50

255ºC ± 5

1.5 - 2.0

alt

 

 

What is the difference between Solder paste and Solder spheres?

Technically, the reflow profiling will be more or less the same as the solder paste SAC305 but will have slight changes due to: 
  • Delivery form - Solder spheres are pre-shaped balls of the solder alloy and solder paste is a pre-mixed suspension of solder particles and flux in a solvent base)
  • Flux impact -  Solder paste relies on the flux to activate cleaning and wetting during soldering. The reflow profile needs to consider the activation and burn-off characteristics of the flux. Solder spheres don't require flux in them internally for reflow.
  • Heating methods: Solder paste is typically heated from the bottom of the PCB during reflow. Solder spheres are often heated from both the top and bottom during reflow, especially for BGA components.  

 

What do I get when I buy SAC305 Solder Spheres from KRAYDEN?

The advantage of ordering solder spheres online at KRAYDEN.com is that you can be sure of the quality. The solder spheres you receive are originally manufactured solder spheres packed into jars with inert gas (nitrogen). We do not repack the solder balls we receive, so the jars you will receive have never been opened, thus ensuring the quality of the product you receive. The lid of the jar is also always sealed with a shrink-wrapped plastic wrap ensuring that the solder spheres do not oxidate in the jar.

 

Description Popular Brand1
Names
Competitive crossovers 
Industry-proven standard Leadfree (Pb-free) Tin Silver Copper (SAC) Solder Spheres. Compare the price and quality of other brands to LINQALLOY SAC305 Solder Spheres
  • Senju Sparkle Ball Sn96.5Ag3Cu0.5
  • Henkel Accurus Sn-Ag3-Cu0.5
  • Nippon Micrometal LF45
  • Cookson Alpha SAC305
  • Indium Precision Spheres 96.5Sn3Ag0.5Cu
  • Kester (EasySpheres) 10-3005
1 Sparkleballs®, Multicore Accurus®, Micrometal®, Precision Spheres®, Alphametal® and Ultra-Spheres® are registered trademarks of Senju, Henkel, NMC, Indium, Cookson and Kester respectively and are not affiliated with this site.



Presentation

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers