LOCTITE ABLESTIK EMI 3620FA

Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category

LOCTITE ABLESTIK EMI 3620FA

Main features

  • Compartment EMI Shielding
  • No popcorning and delamination
  • For gap, hole and trench filling

Product Description

LOCTITE ABLESTIK EMI 3620FA is an electrically conductive adhesive designed for hole, gap or trench filling and for compartment EMI shielding. A package or device manufactured with LOCTITE ABLESTIK EMI 3620FA will exhibit good resistance to delamination and "popcorning" after multiple reflow temperature exposures during reliability testing.

LOCTITE ABLESTIK EMI 3620FA is a solvent free, low viscosity and low outgassing product that is compatible for use with G30 nozzle. This product can be easily applied by dispensing or jetting and is typically used in Sip or newly designed advanced packaging applications.

Cure Schedule

  • 30 mins ramp to 175°C, hold for 60 mins @ 175 °C
  • 30 mins ramp to 150°C, hold 60 mins @ 150 °C
Product Family

233599

4cc in 10cc Syringe - 2449941
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 35 days
Packaging
Unit of measure Syringe
Net weight 15 g
Gross weight 32 g
Dimensions 9.1 x 2.3 x 3 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
8 hours
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
135 °C
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
0.00009 Ohms⋅cm
Physical Properties
Thixotropic index
Thixotropic Index is a ratio of a material s viscosity at two different speeds in Ambient temperature, generally different by a factor of ten. A thixotropic material s viscosity will decrease as agitation or pressure is increased. It indicates the capability of a material to hold its shape. Mayonnaise is a great example of this. It holds its shape very well, but when a shear stress is applied, the material easily spreads. It helps in choosing a material in accordance to the application, dispense method and viscosity of a material.
1.7
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
5,000 mPa.s

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers